NACRES | NB.43 |
General description【一般描述】 | Chemical porcelain has an average coefficient of expansion from 20℃ to 200℃ is 3.56 x 10-6, gradually increasing to 4.69 x 10-6 at 1000℃. To prevent thermal stress cracks on porcelain ware it is strongly recommended a heating/cooling rate not to exceed 200℃/hour. The desiccator plate holes hold crucibles, bottles, or vials, and has a glazed top surface, with feet 16 mm H, for stability. Refractory Qualities Fusion point: 1670℃ Softening point: 1400℃ Limit of use, unglazed: 1400℃ Limit of use, glazed: 1150℃ Limit of use, evacuated: 1300℃ |
产品性质
feature【特点】 | no. of holes 8 |
manufacturer/tradename | Coorstek 60449 |
hole diam.【孔直径】 | 30 mm |